Kalrez 8475 vs Tecnoflon PFR PFR95: FFKM Compound Comparison
Verified by Rachel Mayfield, Supply Chain Analyst - April 2026
Kalrez 8475 and Tecnoflon PFR PFR95 are both perfluoroelastomer (FFKM) compounds used in chemical, refinery, and process applications. Kalrez 8475 vs Tecnoflon PFR PFR95 They share similar chemistry but differ on temperature ceiling, hardness, and intended service. This page compares the two side-by-side and explains when to specify each.
Side-by-side comparison
| Property | Kalrez 8475 | Tecnoflon PFR PFR95 |
|---|---|---|
| Manufacturer | DuPont (Chemours) | Solvay Specialty Polymers |
| Compound | 8475 | PFR95 |
| Maximum continuous temp | 325°C | 250°C |
| Minimum temp | 0°C | -10°C |
| Hardness | 90 Shore A | 90 Shore A |
| Colour | Black | Black |
| Typical applications | Oil and gas downhole, high-pressure valve seats, rapid gas decompression | Higher-pressure valve seats |
When to specify Kalrez 8475
Kalrez 8475 suits oil and gas downhole and similar service. Continuous temperature window is 0°C to 325°C, hardness 90 Shore A. Manufactured by DuPont (Chemours).
When to specify Tecnoflon PFR PFR95
Tecnoflon PFR PFR95 suits higher-pressure valve seats and similar service. Continuous temperature window is -10°C to 250°C, hardness 90 Shore A. Manufactured by Solvay Specialty Polymers.
Key differences
- Temperature ceiling: Kalrez 8475 runs 75°C hotter (325°C vs 250°C). Specify the higher-rated compound when continuous service is above 250°C.
- Hardness: Both are 90 Shore A, so groove design and squeeze percentage are interchangeable.
- Manufacturer: Kalrez 8475 is from DuPont (Chemours); Tecnoflon PFR PFR95 is from Solvay Specialty Polymers. Lead time and UK availability vary by brand.
- Cost: FFKM pricing varies by manufacturer, batch size, and stock position. Both compounds are at the premium end of elastomer pricing (£30 to £500+ per O-ring depending on size).
Get a UK quote on either compound
Related pages
Frequently Asked Questions
Can I substitute Kalrez 8475 for Tecnoflon PFR PFR95?
Yes, Kalrez 8475 and Tecnoflon PFR PFR95 are both FFKM compounds with overlapping chemical compatibility. Verify your specific fluid against both manufacturers' compatibility tables before substitution. Temperature window, hardness, and certifications may differ.
Which is hotter: Kalrez 8475 or Tecnoflon PFR PFR95?
Kalrez 8475 has a higher continuous temperature ceiling (325°C vs 250°C, a 75°C difference).
Which costs less: Kalrez 8475 or Tecnoflon PFR PFR95?
FFKM compound pricing depends on manufacturer, batch size, certifications, and current stock position rather than headline brand. Both compounds are at the premium end of elastomer pricing. Get current UK quotes on both before specifying.
Where can I buy Kalrez 8475 or Tecnoflon PFR PFR95 in the UK?
Both compounds are supplied in the UK by independent FFKM seal specialists carrying multiple manufacturer lines. Lead time is typically 2-5 working days for stock BS 1806 / AS568 sizes, 4-8 weeks for custom-moulded sizes.